{"id":8651,"date":"2026-08-05T18:40:26","date_gmt":"2026-08-06T02:40:26","guid":{"rendered":"https:\/\/fursone.com\/tweed-fabric-weight-gsm-guide\/"},"modified":"2026-09-25T00:47:04","modified_gmt":"2026-09-25T08:47:04","slug":"tweed-fabric-weight-gsm-guide","status":"publish","type":"post","link":"https:\/\/fursone.com\/da\/tweed-fabric-weight-gsm-guide\/","title":{"rendered":"Tweed-stofv\u00e6gtguide: Valg af den rigtige GSM til dit plag"},"content":{"rendered":"<h2>Introduction: Why Tweed Fabric Weight (GSM) Determines Garment Performance<\/h2>\n<p>Tweed fabric weight, measured in grams per square meter (GSM), is the single most important specification when sourcing fabrics for garment production. A 280 GSM tweed produces a structured blazer that holds its shape through daily wear. The same pattern cut from a 550 GSM tweed produces a coat that resists wind and maintains silhouette at sub-zero temperatures. Buy too light and seams pucker, silhouettes collapse, and customers return garments. Buy too heavy and you pay for fabric volume you do not need while creating a garment nobody wears.<\/p>\n<p>At <strong>Fursone Textile<\/strong>, our partner mills in Wenzhou run 300+ looms, producing Chanel-style tweed and woolen overcoat fabrics across a weight range of 280 to 800 GSM. This guide breaks down exactly how to select the right GSM for each garment category, how weight interacts with fiber composition and drape, and how to verify fabric weight before committing to a production run.<\/p>\n<h2>Understanding GSM: What Fabric Weight Actually Measures<\/h2>\n<p>GSM (grams per square meter) quantifies the mass of fabric per unit area. It is distinct from fabric thickness, thread count, and yard weight (ounces per square yard <a href=\"https:\/\/fursone.com\/gsm-to-oz-conversion-fabric-guide\/\" rel=\"noopener\">our GSM to oz\/yd&#178; conversion guide for fabric buyers<\/a>). A high GSM indicates more fiber packed into each square meter, which generally means greater density, better insulation, and more structured drape. However, GSM alone does not predict performance. A 400 GSM wool boucle and a 400 GSM acrylic blend behave differently because fiber composition controls warmth, hand feel, and pilling tendency.<\/p>\n<p>For B2B fabric sourcing, GSM functions as your first filter. Specify GSM before color, before composition, before finish. If you cannot define the target weight range, every downstream decision is guesswork. The table later in this guide maps GSM ranges to garment categories so you can begin sourcing with a defined specification.<\/p>\n<h2>Tweed Fabric Weight Categories: The Four Tiers<\/h2>\n<p>Fabric weight for tweed and overcoat materials divides into four practical tiers. Each tier serves specific garment constructions:<\/p>\n<p><strong>Tier 1: Lightweight (280-350 GSM).<\/strong> Used primarily for Chanel-style tweed blazers, skirt suits, and transitional-season pieces. At this weight, the fabric offers enough body for tailoring without creating a heavy, stiff garment. Our <a href=\"https:\/\/fursone.com\/chanel-style-tweed\/\">Chanel-style tweed<\/a> line spans 280 to 550 GSM, covering this tier and extending into heavier applications.<\/p>\n<p><strong>Tier 2: Midweight (350-450 GSM).<\/strong> The most versatile range. Suitable for structured blazers, suit jackets, and lightweight coats. Fabrics in this range hold shape under linings and interfacing while remaining comfortable for indoor wear. This tier accounts for the majority of Chanel-style tweed production for autumn and spring collections.<\/p>\n<p><strong>Tier 3: Heavyweight (450-550 GSM).<\/strong> Crosses the boundary between jacket and coat territory. At this weight, tweed functions as outerwear. Garments require fewer interlining layers because the fabric provides its own structure. Chanel-style tweed at 500+ GSM produces coats that maintain architectural silhouettes.<\/p>\n<p><strong>Tier 4: Overcoat Grade (550-800 GSM).<\/strong> Dedicated to <a href=\"https:\/\/fursone.com\/woolen-overcoat\/\">woolen overcoat<\/a> production. Wool content ranges from 30% to 80%+. At 800 GSM, a full-length wool coat provides serious winter insulation. These fabrics are dense, wind-resistant, and built for structural garments that hold their shape season after season.<\/p>\n<h2>Jacket and Blazer Weights: Sourcing for Structured Tailoring<\/h2>\n<p>For blazers and suit jackets, the target GSM range is 280 to 450. Within this band, fabric weight must align with the construction method. Fully canvassed jackets require fabric that drapes cleanly over the canvas layer. Unstructured or half-canvas jackets benefit from a heavier fabric that provides its own body.<\/p>\n<p>Key specifications for jacket-weight tweed sourced from Fursone:<\/p>\n<ul>\n<li><strong>GSM range:<\/strong> 280-450 g\/m\u00b2 for Chanel-style tweed blazers<\/li>\n<li><strong>Width:<\/strong> 148-150 cm, maximizing marker efficiency for jacket panels<\/li>\n<li><strong>Pilling resistance:<\/strong> ISO 12945-2 grade 3-4, the standard for garments subjected to friction at cuffs and underarms<\/li>\n<li><strong>Shrinkage control:<\/strong> ISO 6330 compliant, critical because jacket panels fitted to canvas cannot tolerate dimensional change after construction<\/li>\n<li><strong>Color matching:<\/strong> 95% Pantone accuracy across dye lots<\/li>\n<\/ul>\n<p>For multi-piece suit production, source all fabric components from the same dye lot. Fursone maintains re-order consistency at 95%+, meaning subsequent production runs within the same color standard remain within acceptable tolerance for matching.<\/p>\n<h2>Coat Weights: Sourcing for Outerwear Performance<\/h2>\n<p>Coats require a different weight strategy. The fabric functions as the primary insulating layer and structural shell simultaneously. For woolen overcoats, the target range is 450 to 800 GSM.<\/p>\n<p>Within this range, fiber composition becomes a primary variable. At the lower end (450-550 GSM), wool content of 30-50% produces a coat suitable for mild winter climates. At the upper end (650-800 GSM), wool content of 60-80%+ produces a coat rated for sustained cold. The relationship between GSM and wool percentage is not fixed. A 600 GSM fabric with 40% wool will feel different from a 600 GSM fabric with 70% wool. Define both specifications when placing orders.<\/p>\n<p>For knitted overcoat fabrics, shrinkage is the critical metric. Fursone controls knitted overcoat shrinkage to within plus or minus 3%. This tolerance matters because knitted structures are inherently more elastic than woven tweed. If shrinkage exceeds this range, fitted coats distort after the first dry-clean cycle, triggering returns.<\/p>\n<h2>Seasonal Considerations: Matching GSM to Climate and Calendar<\/h2>\n<p>Seasonal collections require calibrated weight selection. The following breakdown maps GSM to seasonal use cases:<\/p>\n<p><strong>Spring (transitional):<\/strong> 280-350 GSM. Chanel-style tweed blazers, lightweight skirts, and shackets. Fabric provides structure without heat retention. Target markets where daytime temperatures range 10 to 20 degrees Celsius.<\/p>\n<p><strong>Summer:<\/strong> Tweed is not a summer-first fabric, but lightweight constructions at 280 GSM work for structured pieces in air-conditioned environments and evening wear. For summer-weight outerwear, consider knitted overcoat constructions at the lower end of the weight range.<\/p>\n<p><strong>Autumn:<\/strong> 350-450 GSM. The peak production season for Chanel-style tweed. Blazers, suit jackets, and lightweight coats. This is the most common weight tier for fashion-forward brands producing structured daywear.<\/p>\n<p><strong>Winter:<\/strong> 450-800 GSM. Full woolen overcoat territory. At 600+ GSM with 60%+ wool content, garments provide genuine insulation for sustained outdoor use. This is where Fursone&#8217;s woolen overcoat line, spanning 450 to 800 GSM with wool content of 30% to 80%+, delivers its core value.<\/p>\n<h2>How to Test and Verify Fabric Weight Before Production<\/h2>\n<p>Specifying GSM on a purchase order does not guarantee the delivered fabric meets that specification. Before committing to a production run, verify weight using standardized methods.<\/p>\n<p><strong>1. Cut and weigh test.<\/strong> Cut a 100 cm by 100 cm sample from the delivered roll. Weigh on a calibrated scale. A 100 cm square sample of 400 GSM fabric should weigh 400 grams. Tolerance of plus or minus 5% is standard industry practice. If the sample weighs 360 grams, you received 360 GSM fabric, not 400 GSM.<\/p>\n<p><strong>2. Wash stability testing.<\/strong> Follow <a href=\"https:\/\/www.iso.org\/standard\/36745.html\" target=\"_blank\" rel=\"noopener\">ISO 6330<\/a> procedures for domestic washing and drying. Measure dimensional change before and after. For knitted overcoat fabrics, confirm shrinkage remains within plus or minus 3%. For woven tweed, confirm the fabric meets the agreed shrinkage specification.<\/p>\n<p><strong>3. Pilling assessment.<\/strong> Test pilling resistance using <a href=\"https:\/\/www.iso.org\/standard\/63549.html\" target=\"_blank\" rel=\"noopener\">ISO 12945-2<\/a> (Martindale method). Fursone fabrics achieve grade 3-4, meaning moderate to good pilling resistance. Grade 5 is the maximum. Garments rated below grade 3 will show visible surface change within a single season of wear.<\/p>\n<p><strong>4. Pantone verification.<\/strong> Compare delivered fabric color to the agreed Pantone reference under D65 daylight simulation. Fursone maintains 95% Pantone accuracy. If the match falls below your tolerance, request a new dye lot before cutting.<\/p>\n<h2>Common Mistakes When Specifying Fabric Weight<\/h2>\n<p>These are the recurring errors we see from buyers:<\/p>\n<p><strong>Mistake 1: Specifying GSM without fiber composition.<\/strong> A 450 GSM fabric with 30% wool and a 450 GSM fabric with 70% wool are not interchangeable. Define both. If the mill substitutes composition to hit a weight target, the garment will not perform as designed.<\/p>\n<p><strong>Mistake 2: Ignoring width.<\/strong> Chanel-style tweed from Fursone runs 148-150 cm wide. Narrower fabrics require more yardage per garment, increasing cost and cutting waste. Always calculate cost per garment, not cost per meter. A wider fabric at a higher per-meter price can produce a lower per-garment cost.<\/p>\n<p><strong>Mistake 3: Treating all overcoat weight as equivalent.<\/strong> The 450-800 GSM range for woolen overcoats is wide. A 480 GSM coat and a 750 GSM coat serve different markets, climates, and price points. Define the target with a 50 GSM window, not the full range.<\/p>\n<p><strong>Mistake 4: Skipping shrinkage testing on knitted fabrics.<\/strong> Knitted overcoat fabrics shrink. If you do not test, you will discover the problem after customer returns arrive. Fursone controls knitted overcoat shrinkage to within plus or minus 3%, but only testing confirms this on your specific order. Mistake 5: Over-ordering on the first run. Fursone&#8217;s MOQ is no minimum for ready stock and 300m per colour for custom development. Start with the stock MOQ to verify the fabric works in your construction before committing to custom production. Re-order consistency sits at 95%+, so scaling up after a successful first run carries low risk.<\/p>\n<h2>Tweed Fabric Weight Guide Table<\/h2>\n<table style=\"border-collapse: collapse; width: 100%; margin: 24px 0;\">\n<thead>\n<tr style=\"background-color: #2c2c2c; color: #ffffff;\">\n<th style=\"border: 1px solid #ddd; padding: 10px; text-align: left;\">GSM Range<\/th>\n<th style=\"border: 1px solid #ddd; padding: 10px; text-align: left;\">Fabric Type<\/th>\n<th style=\"border: 1px solid #ddd; padding: 10px; text-align: left;\">Garment Type<\/th>\n<th style=\"border: 1px solid #ddd; padding: 10px; text-align: left;\">Season<\/th>\n<th style=\"border: 1px solid #ddd; padding: 10px; text-align: left;\">Drape<\/th>\n<\/tr>\n<\/thead>\n<tbody>\n<tr>\n<td style=\"border: 1px solid #ddd; padding: 10px;\">280-350 g\/m\u00b2<\/td>\n<td style=\"border: 1px solid #ddd; padding: 10px;\">Chanel-style tweed<\/td>\n<td style=\"border: 1px solid #ddd; padding: 10px;\">Blazers, skirt suits, shackets<\/td>\n<td style=\"border: 1px solid #ddd; padding: 10px;\">Spring \/ Summer<\/td>\n<td style=\"border: 1px solid #ddd; padding: 10px;\">Soft, fluid<\/td>\n<\/tr>\n<tr>\n<td style=\"border: 1px solid #ddd; padding: 10px;\">350-450 g\/m\u00b2<\/td>\n<td style=\"border: 1px solid #ddd; padding: 10px;\">Chanel-style tweed<\/td>\n<td style=\"border: 1px solid #ddd; padding: 10px;\">Structured blazers, lightweight coats<\/td>\n<td style=\"border: 1px solid #ddd; padding: 10px;\">Autumn<\/td>\n<td style=\"border: 1px solid #ddd; padding: 10px;\">Moderate body<\/td>\n<\/tr>\n<tr>\n<td style=\"border: 1px solid #ddd; padding: 10px;\">450-550 g\/m\u00b2<\/td>\n<td style=\"border: 1px solid #ddd; padding: 10px;\">Chanel-style tweed \/ woolen overcoat<\/td>\n<td style=\"border: 1px solid #ddd; padding: 10px;\">Heavy blazers, transition coats<\/td>\n<td style=\"border: 1px solid #ddd; padding: 10px;\">Autumn \/ Winter<\/td>\n<td style=\"border: 1px solid #ddd; padding: 10px;\">Structured, holds shape<\/td>\n<\/tr>\n<tr>\n<td style=\"border: 1px solid #ddd; padding: 10px;\">550-650 g\/m\u00b2<\/td>\n<td style=\"border: 1px solid #ddd; padding: 10px;\">Woolen overcoat (wool 30-50%+)<\/td>\n<td style=\"border: 1px solid #ddd; padding: 10px;\">Winter coats, peacoats<\/td>\n<td style=\"border: 1px solid #ddd; padding: 10px;\">Winter<\/td>\n<td style=\"border: 1px solid #ddd; padding: 10px;\">Firm, rigid<\/td>\n<\/tr>\n<tr>\n<td style=\"border: 1px solid #ddd; padding: 10px;\">650-800 g\/m\u00b2<\/td>\n<td style=\"border: 1px solid #ddd; padding: 10px;\">Woolen overcoat (wool 60-80%+)<\/td>\n<td style=\"border: 1px solid #ddd; padding: 10px;\">Full-length overcoats, cold-weather coats<\/td>\n<td style=\"border: 1px solid #ddd; padding: 10px;\">Deep Winter<\/td>\n<td style=\"border: 1px solid #ddd; padding: 10px;\">Rigid, sculptural<\/td>\n<\/tr>\n<\/tbody>\n<\/table>\n<p>Fabric width changes yardage more than most buyers expect; our <a href=\"https:\/\/fursone.com\/tweed-fabric-width-58-60-yardage\/\" rel=\"noopener\">tweed fabric width guide<\/a> explains the 58-inch versus 60-inch math.<\/p>\n<h2>Frequently Asked Questions<\/h2>\n<h3>What GSM is best for a Chanel-style tweed blazer?<\/h3>\n<p>The optimal range for a Chanel-style tweed blazer is 280 to 450 GSM. At 280-350 GSM, the blazer will have a softer, more fluid drape suitable for spring collections. At 350-450 GSM, the fabric provides enough body for a fully structured shoulder and clean lapel roll. Specify toward the lower end for unlined or half-lined constructions and toward the upper end for fully canvassed jackets. Fursone&#8217;s Chanel-style tweed line covers the full 280-550 GSM range at 148-150 cm width.<\/p>\n<h3>How does fabric weight affect pilling and durability?<\/h3>\n<p>Higher GSM does not automatically reduce pilling. Pilling resistance depends on fiber composition, yarn twist, and fabric construction. Fursone fabrics meet ISO 12945-2 grade 3-4, tested using the Martindale method, regardless of whether the fabric weighs 280 or 800 GSM. When sourcing, confirm the pilling grade directly rather than assuming that heavier fabric is more durable. A 350 GSM fabric at grade 4 will outperform an 800 GSM fabric at grade 2. What is the minimum order quantity for tweed fabric at Fursone? Ready stock starts from 1 roll with no minimum order quantity, and custom-developed colours start at 300 meters per colour. Stock colors let you test a fabric in your construction before scaling. Custom colors are matched to 95% Pantone accuracy, with re-order consistency at 95%+ across production runs. This means a successful first custom run can be repeated without color drift between batches.<\/p>\n<h3>How do I verify fabric weight before placing a bulk order?<\/h3>\n<p>Request a sample and perform a cut-and-weigh test. Cut a 100 cm square, weigh it on a calibrated scale, and compare to the specified GSM. Tolerance of plus or minus 5% is standard. Additionally, test shrinkage using ISO 6330 procedures and confirm pilling resistance using ISO 12945-2. For knitted overcoat fabrics, verify that shrinkage remains within plus or minus 3% to prevent post-construction distortion.<\/p>\n<h3>How does Fursone&#8217;s pricing compare to European mills?<\/h3>\n<p>Fursone&#8217;s pricing runs at one-fifth to one-third of comparable European mill pricing for equivalent GSM and fiber composition. The cost advantage applies across the full product range, from 280 GSM Chanel-style tweed to 800 GSM woolen overcoat fabric. Certifications including OEKO-TEX, GRS, and SGS apply to production, confirming that the cost difference reflects manufacturing geography rather than reduced quality standards.<\/p>\n<h2>Source the Right Tweed Fabric Weight for Your Collection<\/h2>\n<p>Selecting the correct GSM is the difference between a garment that sells and a garment that gets returned. Define your target weight range, specify fiber composition, verify weight on delivery, and test shrinkage and pilling before cutting. Fursone Textile produces the full spectrum: Chanel-style tweed at 280-550 GSM, woolen overcoat fabric at 450-800 GSM, knitted overcoat fabric with shrinkage controlled to plus or minus 3%, all at 95% Pantone color accuracy and 95%+ re-order consistency.<\/p>\n<p>Stock MOQ is 100 meters. Custom MOQ is 1000 meters per color. Certifications: OEKO-TEX, GRS, SGS. Pricing: one-fifth to one-third of European mills.<\/p>\n<p>Ready to specify fabric for your next production run? <a href=\"https:\/\/fursone.com\/contact\/\">Contact Fursone Textile<\/a> to request samples, confirm GSM availability, and start production. For additional technical questions, see our <a href=\"https:\/\/fursone.com\/faq\/\">FAQ page<\/a> or email <a href=\"mailto:info@fursone.com\">info@fursone.com<\/a> directly.<\/p>\n<p><script type=\"application\/ld+json\">\n{\n  \"@context\": \"https:\/\/schema.org\",\n  \"@type\": \"FAQPage\",\n  \"mainEntity\": [\n    {\n      \"@type\": \"Question\",\n      \"name\": \"What GSM is best for a Chanel-style tweed blazer?\",\n      \"acceptedAnswer\": {\n        \"@type\": \"Answer\",\n        \"text\": \"The optimal range for a Chanel-style tweed blazer is 280 to 450 GSM. At 280-350 GSM, the blazer will have a softer, more fluid drape suitable for spring collections. At 350-450 GSM, the fabric provides enough body for a fully structured shoulder and clean lapel roll. Specify toward the lower end for unlined or half-lined constructions and toward the upper end for fully canvassed jackets. Fursone's Chanel-style tweed line covers the full 280-550 GSM range at 148-150 cm width.\"\n      }\n    },\n    {\n      \"@type\": \"Question\",\n      \"name\": \"How does fabric weight affect pilling and durability?\",\n      \"acceptedAnswer\": {\n        \"@type\": \"Answer\",\n        \"text\": \"Higher GSM does not automatically reduce pilling. Pilling resistance depends on fiber composition, yarn twist, and fabric construction. Fursone fabrics meet ISO 12945-2 grade 3-4, tested using the Martindale method, regardless of whether the fabric weighs 280 or 800 GSM. When sourcing, confirm the pilling grade directly rather than assuming that heavier fabric is more durable. A 350 GSM fabric at grade 4 will outperform an 800 GSM fabric at grade 2.\"\n      }\n    },\n    {\n      \"@type\": \"Question\",\n      \"name\": \"What is the minimum order quantity for tweed fabric at Fursone?\",\n      \"acceptedAnswer\": {\n        \"@type\": \"Answer\",\n        \"text\": \"The MOQ is 100 meters for stock colors and 1000 meters per color for custom-dyed fabric. Stock colors let you test a fabric in your construction before scaling. Custom colors are matched to 95% Pantone accuracy, with re-order consistency at 95%+ across production runs. This means a successful first custom run can be repeated without color drift between batches.\"\n      }\n    },\n    {\n      \"@type\": \"Question\",\n      \"name\": \"How do I verify fabric weight before placing a bulk order?\",\n      \"acceptedAnswer\": {\n        \"@type\": \"Answer\",\n        \"text\": \"Request a sample and perform a cut-and-weigh test. Cut a 100 cm square, weigh it on a calibrated scale, and compare to the specified GSM. Tolerance of plus or minus 5% is standard. Additionally, test shrinkage using ISO 6330 procedures and confirm pilling resistance using ISO 12945-2. For knitted overcoat fabrics, verify that shrinkage remains within plus or minus 3% to prevent post-construction distortion.\"\n      }\n    },\n    {\n      \"@type\": \"Question\",\n      \"name\": \"How does Fursone's pricing compare to European mills?\",\n      \"acceptedAnswer\": {\n        \"@type\": \"Answer\",\n        \"text\": \"Fursone's pricing runs at one-fifth to one-third of comparable European mill pricing for equivalent GSM and fiber composition. The cost advantage applies across the full product range, from 280 GSM Chanel-style tweed to 800 GSM woolen overcoat fabric. Certifications including OEKO-TEX, GRS, and SGS apply to production, confirming that the cost difference reflects manufacturing geography rather than reduced quality standards.\"\n      }\n    }\n  ]\n}\n<\/script><\/p>\n","protected":false},"excerpt":{"rendered":"<p>Introduktion: Hvorfor tweed-stofv\u00e6gt (GSM) afg\u00f8r plaggets ydeevne. Tweed-stofv\u00e6gt, m\u00e5lt i gram pr. kvadratmeter (GSM), er den vigtigste specifikation, n\u00e5r man indk\u00f8ber stoffer til bekl\u00e6dningsproduktion. En tweed p\u00e5 280 GSM giver en struktureret blazer, der holder formen ved daglig brug. Det samme m\u00f8nster sk\u00e5ret i en tweed p\u00e5 550 GSM \u2026 <a title=\"Tweed-stofv\u00e6gtguide: Valg af den rigtige GSM til dit plag\" class=\"read-more\" href=\"https:\/\/fursone.com\/da\/tweed-fabric-weight-gsm-guide\/\" aria-label=\"Read more about Tweed Fabric Weight Guide: Choosing the Right GSM for Your Garment\">L\u00e6s mere <\/a><\/p>","protected":false},"author":1,"featured_media":0,"comment_status":"open","ping_status":"open","sticky":false,"template":"","format":"standard","meta":{"rank_math_title":"","rank_math_description":"","rank_math_focus_keyword":"","rank_math_robots":"","rank_math_canonical_url":"","rank_math_facebook_title":"","rank_math_facebook_description":"","rank_math_twitter_title":"","rank_math_twitter_description":"","_yoast_wpseo_title":"","_yoast_wpseo_metadesc":"","_yoast_wpseo_focuskw":"","_yoast_wpseo_canonical":"","_yoast_wpseo_meta-robots-noindex":"","_yoast_wpseo_meta-robots-nofollow":"","_yoast_wpseo_opengraph-title":"","_yoast_wpseo_opengraph-description":"","_yoast_wpseo_twitter-title":"","_yoast_wpseo_twitter-description":"","_aioseo_title":"","_aioseo_description":"","_aioseo_keywords":"","_aioseo_robots_default":"","_aioseo_robots_noindex":"","_aioseo_og_title":"","_aioseo_og_description":"","_aioseo_twitter_title":"","_aioseo_twitter_description":"","aiosp_title":"","aiosp_description":"","aiosp_keywords":"","_seopress_titles_title":"","_seopress_titles_desc":"","_seopress_analysis_target_kw":"","_seopress_robots_canonical":"","_seopress_robots_index":"","_seopress_robots_follow":"","_seopress_social_fb_title":"","_seopress_social_fb_desc":"","_seopress_social_twitter_title":"","_seopress_social_twitter_desc":"","_genesis_title":"","_genesis_description":"","_genesis_canonical":"","_genesis_noindex":"","_genesis_nofollow":"","slim_seo":"","footnotes":""},"categories":[317],"tags":[],"class_list":["post-8651","post","type-post","status-publish","format-standard","hentry","category-uncategorized"],"_links":{"self":[{"href":"https:\/\/fursone.com\/da\/wp-json\/wp\/v2\/posts\/8651","targetHints":{"allow":["GET"]}}],"collection":[{"href":"https:\/\/fursone.com\/da\/wp-json\/wp\/v2\/posts"}],"about":[{"href":"https:\/\/fursone.com\/da\/wp-json\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"https:\/\/fursone.com\/da\/wp-json\/wp\/v2\/users\/1"}],"replies":[{"embeddable":true,"href":"https:\/\/fursone.com\/da\/wp-json\/wp\/v2\/comments?post=8651"}],"version-history":[{"count":3,"href":"https:\/\/fursone.com\/da\/wp-json\/wp\/v2\/posts\/8651\/revisions"}],"predecessor-version":[{"id":10037,"href":"https:\/\/fursone.com\/da\/wp-json\/wp\/v2\/posts\/8651\/revisions\/10037"}],"wp:attachment":[{"href":"https:\/\/fursone.com\/da\/wp-json\/wp\/v2\/media?parent=8651"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"https:\/\/fursone.com\/da\/wp-json\/wp\/v2\/categories?post=8651"},{"taxonomy":"post_tag","embeddable":true,"href":"https:\/\/fursone.com\/da\/wp-json\/wp\/v2\/tags?post=8651"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}