{"id":10617,"date":"2026-10-02T06:32:05","date_gmt":"2026-10-02T14:32:05","guid":{"rendered":"https:\/\/fursone.com\/mill-visit-what-to-check-sourcing\/"},"modified":"2026-10-02T06:32:05","modified_gmt":"2026-10-02T14:32:05","slug":"mill-visit-what-to-check-sourcing","status":"publish","type":"post","link":"https:\/\/fursone.com\/nl\/mill-visit-what-to-check-sourcing\/","title":{"rendered":"What a Mill Visit Tells You That a Sample Box Cannot"},"content":{"rendered":"<p>Every mill can produce a beautiful sample. The sample is handled by the best operator, on the best loom, with the fibre that happened to be in the sample room that week. The question a buyer actually needs answered is different: what does this mill produce on an ordinary Tuesday, for an order that is not the first one, when the sample room is not watching.<\/p>\n<p>A visit answers that question in a way no sample box can. This guide covers what to look at, what to ask, and what to photograph, so the visit produces evidence instead of impressions.<\/p>\n<p><img decoding=\"async\" class=\"wp-image-2599\" width=\"2560\" height=\"1920\" alt=\"Fabric rolls waiting for inspection before shipment\" src=\"https:\/\/fursone.com\/wp-content\/uploads\/2026\/02\/textile-factory-workshop-production-equipment-manufacturing-fursone-08-1-scaled.jpg\" loading=\"lazy\" srcset=\"https:\/\/fursone.com\/wp-content\/uploads\/2026\/02\/textile-factory-workshop-production-equipment-manufacturing-fursone-08-1-scaled.jpg 2560w, https:\/\/fursone.com\/wp-content\/uploads\/2026\/02\/textile-factory-workshop-production-equipment-manufacturing-fursone-08-1-300x225.jpg 300w, https:\/\/fursone.com\/wp-content\/uploads\/2026\/02\/textile-factory-workshop-production-equipment-manufacturing-fursone-08-1-1024x768.jpg 1024w, https:\/\/fursone.com\/wp-content\/uploads\/2026\/02\/textile-factory-workshop-production-equipment-manufacturing-fursone-08-1-768x576.jpg 768w, https:\/\/fursone.com\/wp-content\/uploads\/2026\/02\/textile-factory-workshop-production-equipment-manufacturing-fursone-08-1-1536x1152.jpg 1536w, https:\/\/fursone.com\/wp-content\/uploads\/2026\/02\/textile-factory-workshop-production-equipment-manufacturing-fursone-08-1-2048x1536.jpg 2048w, https:\/\/fursone.com\/wp-content\/uploads\/2026\/02\/textile-factory-workshop-production-equipment-manufacturing-fursone-08-1-16x12.jpg 16w, https:\/\/fursone.com\/wp-content\/uploads\/2026\/02\/textile-factory-workshop-production-equipment-manufacturing-fursone-08-1-510x382.jpg 510w, https:\/\/fursone.com\/wp-content\/uploads\/2026\/02\/textile-factory-workshop-production-equipment-manufacturing-fursone-08-1-1080x810.jpg 1080w, https:\/\/fursone.com\/wp-content\/uploads\/2026\/02\/textile-factory-workshop-production-equipment-manufacturing-fursone-08-1-1280x960.jpg 1280w, https:\/\/fursone.com\/wp-content\/uploads\/2026\/02\/textile-factory-workshop-production-equipment-manufacturing-fursone-08-1-980x735.jpg 980w, https:\/\/fursone.com\/wp-content\/uploads\/2026\/02\/textile-factory-workshop-production-equipment-manufacturing-fursone-08-1-480x360.jpg 480w\" sizes=\"auto, (max-width: 2560px) 100vw, 2560px\" \/><\/p>\n<h2>Start With Production, Not the Showroom<\/h2>\n<p>The showroom is where visits usually begin and where they reveal the least. Ask to start on the floor instead, and walk the route a real order takes: warping, weaving, inspection, mending, finishing, packing. The route itself is informative, because a mill that cannot walk you through its own order flow in sequence is a mill where orders move by memory rather than by system.<\/p>\n<p>Count the looms and look at what is on them. Are they running the fabric type you are buying, or only plain constructions while your interest is in checks and boucle? A mill with forty looms weaving exactly your construction is a different supplier from one with four hundred looms that will schedule your order wherever a gap appears.<\/p>\n<p>Watch the warping area for size and tension control, and look at how yarn is stored. Humidity and dust in the yarn store predict more about the next order than any brochure, and they are the kind of detail that is only visible in person.<\/p>\n<p><img decoding=\"async\" class=\"wp-image-2602\" width=\"2560\" height=\"1920\" alt=\"Warehouse racks holding wool fabric bales\" src=\"https:\/\/fursone.com\/wp-content\/uploads\/2026\/02\/textile-factory-workshop-production-equipment-manufacturing-fursone-11-1-scaled.jpg\" loading=\"lazy\" srcset=\"https:\/\/fursone.com\/wp-content\/uploads\/2026\/02\/textile-factory-workshop-production-equipment-manufacturing-fursone-11-1-scaled.jpg 2560w, https:\/\/fursone.com\/wp-content\/uploads\/2026\/02\/textile-factory-workshop-production-equipment-manufacturing-fursone-11-1-300x225.jpg 300w, https:\/\/fursone.com\/wp-content\/uploads\/2026\/02\/textile-factory-workshop-production-equipment-manufacturing-fursone-11-1-1024x768.jpg 1024w, https:\/\/fursone.com\/wp-content\/uploads\/2026\/02\/textile-factory-workshop-production-equipment-manufacturing-fursone-11-1-768x576.jpg 768w, https:\/\/fursone.com\/wp-content\/uploads\/2026\/02\/textile-factory-workshop-production-equipment-manufacturing-fursone-11-1-1536x1152.jpg 1536w, https:\/\/fursone.com\/wp-content\/uploads\/2026\/02\/textile-factory-workshop-production-equipment-manufacturing-fursone-11-1-2048x1536.jpg 2048w, https:\/\/fursone.com\/wp-content\/uploads\/2026\/02\/textile-factory-workshop-production-equipment-manufacturing-fursone-11-1-16x12.jpg 16w, https:\/\/fursone.com\/wp-content\/uploads\/2026\/02\/textile-factory-workshop-production-equipment-manufacturing-fursone-11-1-510x382.jpg 510w, https:\/\/fursone.com\/wp-content\/uploads\/2026\/02\/textile-factory-workshop-production-equipment-manufacturing-fursone-11-1-1080x810.jpg 1080w, https:\/\/fursone.com\/wp-content\/uploads\/2026\/02\/textile-factory-workshop-production-equipment-manufacturing-fursone-11-1-1280x960.jpg 1280w, https:\/\/fursone.com\/wp-content\/uploads\/2026\/02\/textile-factory-workshop-production-equipment-manufacturing-fursone-11-1-980x735.jpg 980w, https:\/\/fursone.com\/wp-content\/uploads\/2026\/02\/textile-factory-workshop-production-equipment-manufacturing-fursone-11-1-480x360.jpg 480w\" sizes=\"auto, (max-width: 2560px) 100vw, 2560px\" \/><\/p>\n<h2>The Four Questions That Matter<\/h2>\n<p>First: who owns the looms? Some mills weave everything in-house; others are trading houses that broker to a network of small workshops. Both models can work, but they carry different risks, and the question is the fastest way to learn which model you are talking to.<\/p>\n<p>Second: who does the finishing? Finishing is where fabric quality is won or lost, and many mills send cloth out to a finishing house. Ask which one, ask to see it or at least see its process records, and ask what happens when the finisher is busy in peak season.<\/p>\n<p>Third: how is inspection done? Ask to see the inspection table and the records. A mill that inspects on a backlit frame with a trained inspector and files reports per roll is running a process; a mill that inspects by eye as the roll is wound is running a hope. Fourth: what happens when something goes wrong? Ask for a recent example of a claim, in outline, and what changed afterwards. The answer tells you more about the working relationship than any certification framed on the wall.<\/p>\n<p><img decoding=\"async\" class=\"wp-image-2603\" width=\"2560\" height=\"1920\" alt=\"Packing station where fabric bales are wrapped for export\" src=\"https:\/\/fursone.com\/wp-content\/uploads\/2026\/02\/textile-factory-workshop-production-equipment-manufacturing-fursone-12-1-scaled.jpg\" loading=\"lazy\" srcset=\"https:\/\/fursone.com\/wp-content\/uploads\/2026\/02\/textile-factory-workshop-production-equipment-manufacturing-fursone-12-1-scaled.jpg 2560w, https:\/\/fursone.com\/wp-content\/uploads\/2026\/02\/textile-factory-workshop-production-equipment-manufacturing-fursone-12-1-300x225.jpg 300w, https:\/\/fursone.com\/wp-content\/uploads\/2026\/02\/textile-factory-workshop-production-equipment-manufacturing-fursone-12-1-1024x768.jpg 1024w, https:\/\/fursone.com\/wp-content\/uploads\/2026\/02\/textile-factory-workshop-production-equipment-manufacturing-fursone-12-1-768x576.jpg 768w, https:\/\/fursone.com\/wp-content\/uploads\/2026\/02\/textile-factory-workshop-production-equipment-manufacturing-fursone-12-1-1536x1152.jpg 1536w, https:\/\/fursone.com\/wp-content\/uploads\/2026\/02\/textile-factory-workshop-production-equipment-manufacturing-fursone-12-1-2048x1536.jpg 2048w, https:\/\/fursone.com\/wp-content\/uploads\/2026\/02\/textile-factory-workshop-production-equipment-manufacturing-fursone-12-1-16x12.jpg 16w, https:\/\/fursone.com\/wp-content\/uploads\/2026\/02\/textile-factory-workshop-production-equipment-manufacturing-fursone-12-1-510x382.jpg 510w, https:\/\/fursone.com\/wp-content\/uploads\/2026\/02\/textile-factory-workshop-production-equipment-manufacturing-fursone-12-1-1080x810.jpg 1080w, https:\/\/fursone.com\/wp-content\/uploads\/2026\/02\/textile-factory-workshop-production-equipment-manufacturing-fursone-12-1-1280x960.jpg 1280w, https:\/\/fursone.com\/wp-content\/uploads\/2026\/02\/textile-factory-workshop-production-equipment-manufacturing-fursone-12-1-980x735.jpg 980w, https:\/\/fursone.com\/wp-content\/uploads\/2026\/02\/textile-factory-workshop-production-equipment-manufacturing-fursone-12-1-480x360.jpg 480w\" sizes=\"auto, (max-width: 2560px) 100vw, 2560px\" \/><\/p>\n<h2>Read the Inspection and Mending Stations<\/h2>\n<p>The inspection table is the single most informative object on a mill floor. Look at the lighting, the frame, the record book, and whether the inspector is actually using them. Look at what is stacked beside the table: rejected pieces waiting for a decision, or nothing at all. A mill with no visible rejects is either perfect, or not inspecting.<\/p>\n<p>Mending stations come next. Mending is a skill and a cost, and a mill that invests in it is signalling what kind of quality it intends to ship. Ask to see a mended piece and the corresponding inspection note. How mending is documented tells you whether the mill is managing defects or hiding them.<\/p>\n<p>Packing closes the loop. Watch how bales are wrapped, whether roll numbers are attached, and whether humidity protection is used for humid-season shipments. Packing is where the last two weeks of quality work is protected or lost, and it is one of the few parts of the process that a buyer can change at almost no cost simply by asking. The detailed receiving checks on the other end are covered in <a href=\"https:\/\/fursone.com\/container-arrival-checks-fabric-delivery\/\">container arrival checks<\/a>, which pairs with what you see at this end of the journey.<\/p>\n<h2>Sample From the Running Lot<\/h2>\n<p>The most useful thing to carry home from a visit is not a swatch from the sample room. Ask to cut a small piece from a roll that is running for another customer, subject to their permission, or from the current production of your own reference construction. A piece from a live lot carries the tension, the finishing and the mood of an ordinary production day, which is precisely what you are buying.<\/p>\n<p>Photograph as you go: the looms running your construction, the inspection record page, the mending station, the packing area. These photos become the reference set that later conversations are anchored to. When a batch arrives and something feels different, a photo of the standard you audited is worth more than a description of it.<\/p>\n<p>Finally, write the visit up within a week, while detail is fresh. A one-page record with photos, answers to the four questions and the names of the people you met is the document that turns a pleasant afternoon into usable sourcing evidence. It is also the start of the vendor file that a <a href=\"https:\/\/fursone.com\/fabric-supplier-scorecard-rate-a-vendor\/\">supplier scorecard<\/a> can be built on, and the same file informs the choice between working direct, through an <a href=\"https:\/\/fursone.com\/buying-agent-vs-direct-mill-fabric\/\">agent<\/a> or in some combination.<\/p>\n<h2>After the Visit: Turning Impressions Into Decisions<\/h2>\n<p>A visit produces three kinds of information: facts you can verify later, impressions that need to be tested, and gaps you could not close on the day. Sort them that way when you write up. The facts go into the vendor file; the impressions become the questions for the next call; the gaps become the reasons for a second visit or a reference check.<\/p>\n<p>Use the visit to set the specification, not just to judge the supplier. If the mill&#8217;s strength is a construction outside your current brief, and the price of that construction is acceptable, the visit has earned its cost. Buyers who visit with an open brief consistently find one or two opportunities they would have missed on paper.<\/p>\n<p>Finally, check the market context before you go. The country commercial guides published by the <a href=\"https:\/\/www.trade.gov\/country-commercial-guides\" target=\"_blank\" rel=\"noopener\">US Commercial Service<\/a> cover business practice, documentation and market conditions per country, and reading the relevant guide before the trip turns a set of general impressions into specific questions. Our own <a href=\"https:\/\/fursone.com\/fabric-sourcing-guide\/\">fabric sourcing guide<\/a> sets out the same process from the enquiry side, and the two are designed to be used in the same sequence.<\/p>\n<h2>FAQ<\/h2>\n<div class=\"faq-card\" style=\"background:#f9f9f9;border-left:4px solid #333;padding:1.2em 1.5em;margin-bottom:1em;\">\n<h3 style=\"font-size:1.1em;margin:0 0 0.5em;\">What is the single most useful thing to see on a mill visit?<\/h3>\n<p style=\"font-size:15px;line-height:1.7;margin:0;\">The inspection table and its records. It shows whether quality is a process or a promise.<\/p>\n<\/div>\n<div class=\"faq-card\" style=\"background:#f9f9f9;border-left:4px solid #333;padding:1.2em 1.5em;margin-bottom:1em;\">\n<h3 style=\"font-size:1.1em;margin:0 0 0.5em;\">Should I take samples from the sample room?<\/h3>\n<p style=\"font-size:15px;line-height:1.7;margin:0;\">Ask for a piece from a running production lot instead. It reflects an ordinary day rather than a prepared sample.<\/p>\n<\/div>\n<div class=\"faq-card\" style=\"background:#f9f9f9;border-left:4px solid #333;padding:1.2em 1.5em;margin-bottom:1em;\">\n<h3 style=\"font-size:1.1em;margin:0 0 0.5em;\">How do I know if a mill subcontracts weaving?<\/h3>\n<p style=\"font-size:15px;line-height:1.7;margin:0;\">Ask directly who owns the looms and where the fabric is woven. Ask to see the weaving floor for your construction.<\/p>\n<\/div>\n<div class=\"faq-card\" style=\"background:#f9f9f9;border-left:4px solid #333;padding:1.2em 1.5em;margin-bottom:1em;\">\n<h3 style=\"font-size:1.1em;margin:0 0 0.5em;\">What should I photograph?<\/h3>\n<p style=\"font-size:15px;line-height:1.7;margin:0;\">Looms running your construction, inspection records, the mending station and the packing area, all with permission.<\/p>\n<\/div>\n<div class=\"faq-card\" style=\"background:#f9f9f9;border-left:4px solid #333;padding:1.2em 1.5em;margin-bottom:1em;\">\n<h3 style=\"font-size:1.1em;margin:0 0 0.5em;\">How soon should the visit be written up?<\/h3>\n<p style=\"font-size:15px;line-height:1.7;margin:0;\">Within a week, as a one-page record with photos, answers and names. It becomes the vendor file.<\/p>\n<\/div>\n<h2>Video: High-Quality Fabrics for Designers: My Journey<\/h2>\n<div class=\"yt-facade\" data-yt-id=\"qwHW9EY2cdk\" role=\"button\" tabindex=\"0\" aria-label=\"Play video: High-Quality Fabrics for Designers: My Journey\" style=\"position:relative;padding-bottom:56.25%;height:0;overflow:hidden;margin:2em 0;background:#1a1a1a;cursor:pointer;\"><span style=\"position:absolute;top:50%;left:50%;transform:translate(-50%,-50%);width:72px;height:72px;border-radius:50%;background:rgba(255,255,255,0.92);display:flex;align-items:center;justify-content:center;font-size:26px;color:#111;line-height:1;\">&#9654;<\/span><span style=\"position:absolute;left:16px;right:16px;bottom:14px;color:#fff;font-size:14px;line-height:1.45;\">High-Quality Fabrics for Designers: My Journey<\/span><\/div>\n<p><script>\n(function(){var f=document.querySelector('.yt-facade');if(!f){return;}f.addEventListener('click',function(){var id=f.getAttribute('data-yt-id');f.innerHTML='<iframe style=\"position:absolute;top:0;left:0;width:100%;height:100%;\" src=\"https:\/\/www.youtube.com\/embed\/'+id+'?autoplay=1\" title=\"YouTube video player\" frameborder=\"0\" allow=\"accelerometer;autoplay;clipboard-write;encrypted-media;gyroscope;picture-in-picture\" allowfullscreen data-no-lzy loading=\"eager\"><\/iframe>';});})();\n<\/script><\/p>\n<p>If you are planning a sourcing trip or deciding whether a mill is worth one, our <a href=\"https:\/\/fursone.com\/fabric-sourcing-guide\/\">fabric sourcing guide<\/a> sets out the questions to bring and the evidence to collect, and the team can host a visit against the same checklist.<\/p>\n<p><script type=\"application\/ld+json\" id=\"evo301-geo-ai-block\">\n{\n  \"@context\": \"https:\/\/schema.org\",\n  \"@type\": \"DefinedTermSet\",\n  \"name\": \"Fabric Mill Visits\",\n  \"description\": \"A mill visit verifies what a sample cannot: production on an ordinary day. The useful route runs warping, weaving, inspection, mending, finishing and packing, with four questions asked directly: who owns the looms, who does the finishing, how inspection is recorded, and what happens when something goes wrong. The most useful sample is a piece cut from a running production lot.\",\n  \"dataStatement\": [\n    \"Walk the order route: warping, weaving, inspection, mending, finishing, packing.\",\n    \"Four questions: loom ownership, finishing partner, inspection records, claim history.\",\n    \"A live-lot sample substitutes for a prepared swatch.\"\n  ],\n  \"qaConcise\": [\n    {\n      \"question\": \"What does a visit reveal that samples do not?\",\n      \"answer\": \"Daily process control: inspection discipline, mending, packing and answers about subcontracting.\"\n    },\n    {\n      \"question\": \"Which station matters most?\",\n      \"answer\": \"The inspection table and its records.\"\n    },\n    {\n      \"question\": \"How is the visit documented?\",\n      \"answer\": \"A one-page record with photos and the four answers, written within a week and filed as vendor evidence.\"\n    }\n  ]\n}\n<\/script><\/p>\n<p><script type=\"application\/ld+json\">\n{\n  \"@context\": \"https:\/\/schema.org\",\n  \"@type\": \"FAQPage\",\n  \"mainEntity\": [\n    {\n      \"@type\": \"Question\",\n      \"name\": \"What is the single most useful thing to see on a mill visit?\",\n      \"acceptedAnswer\": {\n        \"@type\": \"Answer\",\n        \"text\": \"The inspection table and its records. It shows whether quality is a process or a promise.\"\n      }\n    },\n    {\n      \"@type\": \"Question\",\n      \"name\": \"Should I take samples from the sample room?\",\n      \"acceptedAnswer\": {\n        \"@type\": \"Answer\",\n        \"text\": \"Ask for a piece from a running production lot instead. It reflects an ordinary day rather than a prepared sample.\"\n      }\n    },\n    {\n      \"@type\": \"Question\",\n      \"name\": \"How do I know if a mill subcontracts weaving?\",\n      \"acceptedAnswer\": {\n        \"@type\": \"Answer\",\n        \"text\": \"Ask directly who owns the looms and where the fabric is woven. Ask to see the weaving floor for your construction.\"\n      }\n    },\n    {\n      \"@type\": \"Question\",\n      \"name\": \"What should I photograph?\",\n      \"acceptedAnswer\": {\n        \"@type\": \"Answer\",\n        \"text\": \"Looms running your construction, inspection records, the mending station and the packing area, all with permission.\"\n      }\n    },\n    {\n      \"@type\": \"Question\",\n      \"name\": \"How soon should the visit be written up?\",\n      \"acceptedAnswer\": {\n        \"@type\": \"Answer\",\n        \"text\": \"Within a week, as a one-page record with photos, answers and names. It becomes the vendor file.\"\n      }\n    }\n  ]\n}\n<\/script><\/p>\n","protected":false},"excerpt":{"rendered":"<p>Every mill can produce a beautiful sample. The sample is handled by the best operator, on the best loom, with the fibre that happened to be in the sample room that week. The question a buyer actually needs answered is different: what does this mill produce on an ordinary Tuesday, for an order that is &#8230; <a title=\"What a Mill Visit Tells You That a Sample Box Cannot\" class=\"read-more\" href=\"https:\/\/fursone.com\/nl\/mill-visit-what-to-check-sourcing\/\" aria-label=\"Lees meer over What a Mill Visit Tells You That a Sample Box Cannot\">Lees verder<\/a><\/p>","protected":false},"author":1,"featured_media":2598,"comment_status":"open","ping_status":"open","sticky":false,"template":"","format":"standard","meta":{"rank_math_title":"Fabric Mill Visit Checklist | What Samples Cannot Show You","rank_math_description":"A sample box shows what a mill can do once. A visit shows how it does it every day: looms, inspection, finishing, packing and the answers to four questions.","rank_math_focus_keyword":"fabric mill visit checklist","rank_math_robots":"","rank_math_canonical_url":"","rank_math_facebook_title":"","rank_math_facebook_description":"","rank_math_twitter_title":"","rank_math_twitter_description":"","_yoast_wpseo_title":"","_yoast_wpseo_metadesc":"","_yoast_wpseo_focuskw":"","_yoast_wpseo_canonical":"","_yoast_wpseo_meta-robots-noindex":"","_yoast_wpseo_meta-robots-nofollow":"","_yoast_wpseo_opengraph-title":"","_yoast_wpseo_opengraph-description":"","_yoast_wpseo_twitter-title":"","_yoast_wpseo_twitter-description":"","_aioseo_title":"","_aioseo_description":"","_aioseo_keywords":"","_aioseo_robots_default":"","_aioseo_robots_noindex":"","_aioseo_og_title":"","_aioseo_og_description":"","_aioseo_twitter_title":"","_aioseo_twitter_description":"","aiosp_title":"","aiosp_description":"","aiosp_keywords":"","_seopress_titles_title":"","_seopress_titles_desc":"","_seopress_analysis_target_kw":"","_seopress_robots_canonical":"","_seopress_robots_index":"","_seopress_robots_follow":"","_seopress_social_fb_title":"","_seopress_social_fb_desc":"","_seopress_social_twitter_title":"","_seopress_social_twitter_desc":"","_genesis_title":"","_genesis_description":"","_genesis_canonical":"","_genesis_noindex":"","_genesis_nofollow":"","slim_seo":"","footnotes":""},"categories":[312],"tags":[],"class_list":["post-10617","post","type-post","status-publish","format-standard","has-post-thumbnail","hentry","category-sourcing-guide"],"_links":{"self":[{"href":"https:\/\/fursone.com\/nl\/wp-json\/wp\/v2\/posts\/10617","targetHints":{"allow":["GET"]}}],"collection":[{"href":"https:\/\/fursone.com\/nl\/wp-json\/wp\/v2\/posts"}],"about":[{"href":"https:\/\/fursone.com\/nl\/wp-json\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"https:\/\/fursone.com\/nl\/wp-json\/wp\/v2\/users\/1"}],"replies":[{"embeddable":true,"href":"https:\/\/fursone.com\/nl\/wp-json\/wp\/v2\/comments?post=10617"}],"version-history":[{"count":0,"href":"https:\/\/fursone.com\/nl\/wp-json\/wp\/v2\/posts\/10617\/revisions"}],"wp:featuredmedia":[{"embeddable":true,"href":"https:\/\/fursone.com\/nl\/wp-json\/wp\/v2\/media\/2598"}],"wp:attachment":[{"href":"https:\/\/fursone.com\/nl\/wp-json\/wp\/v2\/media?parent=10617"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"https:\/\/fursone.com\/nl\/wp-json\/wp\/v2\/categories?post=10617"},{"taxonomy":"post_tag","embeddable":true,"href":"https:\/\/fursone.com\/nl\/wp-json\/wp\/v2\/tags?post=10617"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}