{"id":10616,"date":"2026-10-02T06:31:53","date_gmt":"2026-10-02T14:31:53","guid":{"rendered":"https:\/\/fursone.com\/raising-brushing-nap-finishing\/"},"modified":"2026-10-02T06:31:53","modified_gmt":"2026-10-02T14:31:53","slug":"raising-brushing-nap-finishing","status":"publish","type":"post","link":"https:\/\/fursone.com\/sv\/raising-brushing-nap-finishing\/","title":{"rendered":"Raising and Brushing: How Nap Is Built in Wool Finishing"},"content":{"rendered":"<p>Two wool fabrics can leave the loom identical and arrive as different products. One is flat with the weave clearly readable, the other carries a soft surface where the structure sits behind a veil of fibre. The difference is not the yarn and not the weave; it is a pair of finishing steps, raising and brushing, that pull fibre to the surface and lay it into a direction.<\/p>\n<p>This guide covers what those steps do, where they sit in the finishing sequence, how nap direction affects cutting, and the point at which raising stops improving a cloth and starts weakening it.<\/p>\n<p><img decoding=\"async\" class=\"wp-image-2249\" width=\"2560\" height=\"1920\" alt=\"Brushing and raising machine area in the finishing hall\" src=\"https:\/\/fursone.com\/wp-content\/uploads\/2026\/02\/textile-factory-workshop-production-equipment-manufacturing-fursone-38-scaled.jpg\" loading=\"lazy\" srcset=\"https:\/\/fursone.com\/wp-content\/uploads\/2026\/02\/textile-factory-workshop-production-equipment-manufacturing-fursone-38-scaled.jpg 2560w, https:\/\/fursone.com\/wp-content\/uploads\/2026\/02\/textile-factory-workshop-production-equipment-manufacturing-fursone-38-300x225.jpg 300w, https:\/\/fursone.com\/wp-content\/uploads\/2026\/02\/textile-factory-workshop-production-equipment-manufacturing-fursone-38-1024x768.jpg 1024w, https:\/\/fursone.com\/wp-content\/uploads\/2026\/02\/textile-factory-workshop-production-equipment-manufacturing-fursone-38-768x576.jpg 768w, https:\/\/fursone.com\/wp-content\/uploads\/2026\/02\/textile-factory-workshop-production-equipment-manufacturing-fursone-38-1536x1152.jpg 1536w, https:\/\/fursone.com\/wp-content\/uploads\/2026\/02\/textile-factory-workshop-production-equipment-manufacturing-fursone-38-2048x1536.jpg 2048w, https:\/\/fursone.com\/wp-content\/uploads\/2026\/02\/textile-factory-workshop-production-equipment-manufacturing-fursone-38-16x12.jpg 16w, https:\/\/fursone.com\/wp-content\/uploads\/2026\/02\/textile-factory-workshop-production-equipment-manufacturing-fursone-38-510x382.jpg 510w, https:\/\/fursone.com\/wp-content\/uploads\/2026\/02\/textile-factory-workshop-production-equipment-manufacturing-fursone-38-1080x810.jpg 1080w, https:\/\/fursone.com\/wp-content\/uploads\/2026\/02\/textile-factory-workshop-production-equipment-manufacturing-fursone-38-1280x960.jpg 1280w, https:\/\/fursone.com\/wp-content\/uploads\/2026\/02\/textile-factory-workshop-production-equipment-manufacturing-fursone-38-980x735.jpg 980w, https:\/\/fursone.com\/wp-content\/uploads\/2026\/02\/textile-factory-workshop-production-equipment-manufacturing-fursone-38-480x360.jpg 480w\" sizes=\"auto, (max-width: 2560px) 100vw, 2560px\" \/><\/p>\n<h2>What Raising Does to a Woven Cloth<\/h2>\n<p>Raising, also called napping, passes the fabric over rollers covered in fine wire teeth that tease fibres out of the yarn structure and up to the surface. The result is a nap: a layer of loose fibre standing above the weave. Done lightly, it gives a flannel-like softness while the pattern stays visible; done heavily, it produces the dense surface associated with blankets and heavy coating cloth.<\/p>\n<p>Brushing follows or accompanies raising, using softer brushes to lift the fibre into a consistent direction and remove loose material. Raising creates the nap; brushing decides how it lies. A brushed finish is what gives certain woollen cloths their characteristic smooth, directional hand.<\/p>\n<p>Both steps change the measurable properties of the fabric. Surface weight increases because fibre that was inside the yarn now stands above it. Thermal insulation improves because the trapped air layer grows. Tear strength usually falls, because the fibres that were contributing to yarn integrity have been pulled partly out of the structure.<\/p>\n<h2>Where the Steps Sit in the Finishing Line<\/h2>\n<p>Raising belongs after fulling and before the final pressing and decatizing steps. Fulling, the controlled wet milling that makes wool felt and shrink, sets the body of the cloth; raising then works on that stabilised structure. Sequence matters because raising a cloth that has not been fully stabilised produces an uneven nap that will not survive the later wet steps.<\/p>\n<p>After raising comes shearing, also called cropping, where rotating blades cut the nap to a uniform height. Shearing is what turns a rough raised surface into a controlled one, and it is where the difference between a cheap and an expensive raised cloth usually lives: one pass or three, freshly sharpened blades or worn ones, an even cut or a patchy one.<\/p>\n<p>The line ends with the stability and hand steps. The fuller picture of how these finishing stages work together, including the steps that come before raising, is set out in our notes on <a href=\"https:\/\/fursone.com\/fulling-finishing-tweed-hand-feel\/\">fulling and finishing for tweed<\/a> and on <a href=\"https:\/\/fursone.com\/decatizing-crabbing-tweed-finishing\/\">decatizing and crabbing<\/a>, which are the two references worth reading together with this one.<\/p>\n<p><img decoding=\"async\" class=\"wp-image-2596\" width=\"2560\" height=\"1920\" alt=\"Warping section preparing yarn beams for weaving\" src=\"https:\/\/fursone.com\/wp-content\/uploads\/2026\/02\/textile-factory-workshop-production-equipment-manufacturing-fursone-05-1-scaled.jpg\" loading=\"lazy\" srcset=\"https:\/\/fursone.com\/wp-content\/uploads\/2026\/02\/textile-factory-workshop-production-equipment-manufacturing-fursone-05-1-scaled.jpg 2560w, https:\/\/fursone.com\/wp-content\/uploads\/2026\/02\/textile-factory-workshop-production-equipment-manufacturing-fursone-05-1-300x225.jpg 300w, https:\/\/fursone.com\/wp-content\/uploads\/2026\/02\/textile-factory-workshop-production-equipment-manufacturing-fursone-05-1-1024x768.jpg 1024w, https:\/\/fursone.com\/wp-content\/uploads\/2026\/02\/textile-factory-workshop-production-equipment-manufacturing-fursone-05-1-768x576.jpg 768w, https:\/\/fursone.com\/wp-content\/uploads\/2026\/02\/textile-factory-workshop-production-equipment-manufacturing-fursone-05-1-1536x1152.jpg 1536w, https:\/\/fursone.com\/wp-content\/uploads\/2026\/02\/textile-factory-workshop-production-equipment-manufacturing-fursone-05-1-2048x1536.jpg 2048w, https:\/\/fursone.com\/wp-content\/uploads\/2026\/02\/textile-factory-workshop-production-equipment-manufacturing-fursone-05-1-16x12.jpg 16w, https:\/\/fursone.com\/wp-content\/uploads\/2026\/02\/textile-factory-workshop-production-equipment-manufacturing-fursone-05-1-510x382.jpg 510w, https:\/\/fursone.com\/wp-content\/uploads\/2026\/02\/textile-factory-workshop-production-equipment-manufacturing-fursone-05-1-1080x810.jpg 1080w, https:\/\/fursone.com\/wp-content\/uploads\/2026\/02\/textile-factory-workshop-production-equipment-manufacturing-fursone-05-1-1280x960.jpg 1280w, https:\/\/fursone.com\/wp-content\/uploads\/2026\/02\/textile-factory-workshop-production-equipment-manufacturing-fursone-05-1-980x735.jpg 980w, https:\/\/fursone.com\/wp-content\/uploads\/2026\/02\/textile-factory-workshop-production-equipment-manufacturing-fursone-05-1-480x360.jpg 480w\" sizes=\"auto, (max-width: 2560px) 100vw, 2560px\" \/><\/p>\n<h2>Nap Direction: The Detail That Reaches the Cutting Table<\/h2>\n<p>A raised cloth has a direction. Run a hand along the nap and it feels smooth in one direction and rough in the other, and under light the same piece reads lighter or darker depending on which way the pile lies. This is not a defect; it is the nature of a directional surface, and it is why raised fabrics must be cut with all pattern pieces laid in the same direction.<\/p>\n<p>When direction is ignored, panels sewn together face different ways and the garment shows a colour shift at the seam that no amount of pressing removes. The fault looks like a dyeing problem and is actually a cutting problem, and it is one of the most common causes of a raised-fabric programme failing at the sample stage.<\/p>\n<p>The practical controls are simple. Mark the nap direction on the fabric with an arrow at the mill, state the direction convention in the cut sheet, and require the cutting room to confirm it on the first lay of every bale. Buyers who also plan a <a href=\"https:\/\/fursone.com\/fabric-hand-feel-test\/\">hand feel test<\/a> as part of incoming checks get a quick read on whether the surface matches the approved standard, because nap direction is easiest to feel before it is easiest to see.<\/p>\n<p><img decoding=\"async\" class=\"wp-image-2597\" width=\"2560\" height=\"1920\" alt=\"Mill technician checking fabric on the loom\" src=\"https:\/\/fursone.com\/wp-content\/uploads\/2026\/02\/textile-factory-workshop-production-equipment-manufacturing-fursone-06-1-scaled.jpg\" loading=\"lazy\" srcset=\"https:\/\/fursone.com\/wp-content\/uploads\/2026\/02\/textile-factory-workshop-production-equipment-manufacturing-fursone-06-1-scaled.jpg 2560w, https:\/\/fursone.com\/wp-content\/uploads\/2026\/02\/textile-factory-workshop-production-equipment-manufacturing-fursone-06-1-300x225.jpg 300w, https:\/\/fursone.com\/wp-content\/uploads\/2026\/02\/textile-factory-workshop-production-equipment-manufacturing-fursone-06-1-1024x768.jpg 1024w, https:\/\/fursone.com\/wp-content\/uploads\/2026\/02\/textile-factory-workshop-production-equipment-manufacturing-fursone-06-1-768x576.jpg 768w, https:\/\/fursone.com\/wp-content\/uploads\/2026\/02\/textile-factory-workshop-production-equipment-manufacturing-fursone-06-1-1536x1152.jpg 1536w, https:\/\/fursone.com\/wp-content\/uploads\/2026\/02\/textile-factory-workshop-production-equipment-manufacturing-fursone-06-1-2048x1536.jpg 2048w, https:\/\/fursone.com\/wp-content\/uploads\/2026\/02\/textile-factory-workshop-production-equipment-manufacturing-fursone-06-1-16x12.jpg 16w, https:\/\/fursone.com\/wp-content\/uploads\/2026\/02\/textile-factory-workshop-production-equipment-manufacturing-fursone-06-1-510x382.jpg 510w, https:\/\/fursone.com\/wp-content\/uploads\/2026\/02\/textile-factory-workshop-production-equipment-manufacturing-fursone-06-1-1080x810.jpg 1080w, https:\/\/fursone.com\/wp-content\/uploads\/2026\/02\/textile-factory-workshop-production-equipment-manufacturing-fursone-06-1-1280x960.jpg 1280w, https:\/\/fursone.com\/wp-content\/uploads\/2026\/02\/textile-factory-workshop-production-equipment-manufacturing-fursone-06-1-980x735.jpg 980w, https:\/\/fursone.com\/wp-content\/uploads\/2026\/02\/textile-factory-workshop-production-equipment-manufacturing-fursone-06-1-480x360.jpg 480w\" sizes=\"auto, (max-width: 2560px) 100vw, 2560px\" \/><\/p>\n<h2>The Risks of Raising Too Far<\/h2>\n<p>Raising has a point of diminishing returns and a point of damage. Over-raised cloth loses tear strength, pills more readily because loose fibre migrates, and sheds in use, which matters most for garments that will be worn against other fabrics. In extreme cases the surface looks full but the cloth feels spongy and unsupportive.<\/p>\n<p>Shade is the second casualty. Raising lifts fibre that may sit differently from the base cloth, so a heavily raised piece can appear lighter or greyer than the approved swatch even though the yarn lot is unchanged. Buyers approving a raised fabric from a swatch should confirm that the swatch itself is a raised piece from the same finishing line, not a loom-state sample with a promise attached.<\/p>\n<p>Both properties are testable. Pilling resistance is assessed with standard abrasion tests, and the <a href=\"https:\/\/www.iso.org\/standards.html\" target=\"_blank\" rel=\"noopener\">ISO standards library<\/a> indexes the textile test methods, including the pilling and abrasion families, that mills and third-party labs work from. Writing a pilling requirement into a raised-fabric order is the cheapest way to keep the surface from degrading in the first weeks of wear.<\/p>\n<h2>Specifying a Raised Finish<\/h2>\n<p>A workable specification names the finish rather than describing it: single or double raised, one face or both, nap direction and its marking convention, and the shearing standard with a reference sample. Then it names the tests: pilling resistance, and where relevant, dimensional stability after the finishing sequence.<\/p>\n<p>The reference sample is what prevents drift. Keep a finished piece from the approval round, sealed and dated, and compare each subsequent bale against it by hand and by eye under the same lighting. Raised surfaces are forgiving in photographs and unforgiving in person.<\/p>\n<p>Finally, decide the commercial consequence of a nap that is close but not equal. On a solid-colour line the tolerance can be wide; on a programme where raised and flat panels sit together, it is narrow by definition. The manufacturing side of that decision, from finishing trials to bulk finishing control, is part of the <a href=\"https:\/\/fursone.com\/custom-manufacturing\/\">custom fabric manufacturing service<\/a> we run, and finishing settings are agreed with the buyer before the first bulk lot enters the line.<\/p>\n<h2>FAQ<\/h2>\n<div class=\"faq-card\" style=\"background:#f9f9f9;border-left:4px solid #333;padding:1.2em 1.5em;margin-bottom:1em;\">\n<h3 style=\"font-size:1.1em;margin:0 0 0.5em;\">What is the difference between raising and brushing?<\/h3>\n<p style=\"font-size:15px;line-height:1.7;margin:0;\">Raising teases fibre out of the yarn with wire-covered rollers to create nap. Brushing lifts and aligns that nap and clears loose fibre.<\/p>\n<\/div>\n<div class=\"faq-card\" style=\"background:#f9f9f9;border-left:4px solid #333;padding:1.2em 1.5em;margin-bottom:1em;\">\n<h3 style=\"font-size:1.1em;margin:0 0 0.5em;\">Where does raising sit in the finishing line?<\/h3>\n<p style=\"font-size:15px;line-height:1.7;margin:0;\">After fulling, before shearing and the final stability steps such as pressing or decatizing.<\/p>\n<\/div>\n<div class=\"faq-card\" style=\"background:#f9f9f9;border-left:4px solid #333;padding:1.2em 1.5em;margin-bottom:1em;\">\n<h3 style=\"font-size:1.1em;margin:0 0 0.5em;\">Why must all panels be cut in one direction?<\/h3>\n<p style=\"font-size:15px;line-height:1.7;margin:0;\">A raised surface is directional. Panels cut in opposite directions reflect light differently and show a colour shift at the seam.<\/p>\n<\/div>\n<div class=\"faq-card\" style=\"background:#f9f9f9;border-left:4px solid #333;padding:1.2em 1.5em;margin-bottom:1em;\">\n<h3 style=\"font-size:1.1em;margin:0 0 0.5em;\">Does raising weaken the fabric?<\/h3>\n<p style=\"font-size:15px;line-height:1.7;margin:0;\">It reduces tear strength and can increase pilling, because fibre that supported the yarn structure is lifted to the surface.<\/p>\n<\/div>\n<div class=\"faq-card\" style=\"background:#f9f9f9;border-left:4px solid #333;padding:1.2em 1.5em;margin-bottom:1em;\">\n<h3 style=\"font-size:1.1em;margin:0 0 0.5em;\">How is a raised finish specified?<\/h3>\n<p style=\"font-size:15px;line-height:1.7;margin:0;\">By finish type and passes, faces, nap direction and shearing standard, plus a sealed reference sample and a pilling test requirement.<\/p>\n<\/div>\n<h2>Video: Tweed Fabric: Innovations and Highlights from a Leading Manufacturer<\/h2>\n<div class=\"yt-facade\" data-yt-id=\"_3QFhfUVug0\" role=\"button\" tabindex=\"0\" aria-label=\"Play video: Tweed Fabric: Innovations and Highlights from a Leading Manufacturer\" style=\"position:relative;padding-bottom:56.25%;height:0;overflow:hidden;margin:2em 0;background:#1a1a1a;cursor:pointer;\"><span style=\"position:absolute;top:50%;left:50%;transform:translate(-50%,-50%);width:72px;height:72px;border-radius:50%;background:rgba(255,255,255,0.92);display:flex;align-items:center;justify-content:center;font-size:26px;color:#111;line-height:1;\">&#9654;<\/span><span style=\"position:absolute;left:16px;right:16px;bottom:14px;color:#fff;font-size:14px;line-height:1.45;\">Tweed Fabric: Innovations and Highlights from a Leading Manufacturer<\/span><\/div>\n<p><script>\n(function(){var f=document.querySelector('.yt-facade');if(!f){return;}f.addEventListener('click',function(){var id=f.getAttribute('data-yt-id');f.innerHTML='<iframe style=\"position:absolute;top:0;left:0;width:100%;height:100%;\" src=\"https:\/\/www.youtube.com\/embed\/'+id+'?autoplay=1\" title=\"YouTube video player\" frameborder=\"0\" allow=\"accelerometer;autoplay;clipboard-write;encrypted-media;gyroscope;picture-in-picture\" allowfullscreen data-no-lzy loading=\"eager\"><\/iframe>';});})();\n<\/script><\/p>\n<p>If a raised or brushed surface is central to your line, agree the finish and its tests before the first bulk lot. The <a href=\"https:\/\/fursone.com\/custom-manufacturing\/\">custom fabric manufacturing service<\/a> runs finishing trials, keeps a sealed reference and documents the settings that produced it, so batch two arrives looking like batch one.<\/p>\n<p><script type=\"application\/ld+json\" id=\"evo301-geo-ai-block\">\n{\n  \"@context\": \"https:\/\/schema.org\",\n  \"@type\": \"DefinedTermSet\",\n  \"name\": \"Raising and Brushing in Wool Finishing\",\n  \"description\": \"Raising (napping) pulls fibres from the yarn structure to the surface using wire-covered rollers; brushing aligns the resulting nap and removes loose fibre. In wool finishing, raising follows fulling and precedes shearing and decatizing. The result adds warmth and softness, reduces weave definition, lowers tear strength, and creates a directional surface that must be cut in a single direction.\",\n  \"dataStatement\": [\n    \"Finishing sequence: fulling, raising, shearing, pressing or decatizing.\",\n    \"Nap direction must be marked and respected at the cutting table.\",\n    \"Pilling and abrasion resistance are assessed with standard textile test methods indexed by ISO.\"\n  ],\n  \"qaConcise\": [\n    {\n      \"question\": \"What does raising add?\",\n      \"answer\": \"Surface nap: softness, warmth and cover, at the cost of some tear strength and weave definition.\"\n    },\n    {\n      \"question\": \"Why does nap direction matter?\",\n      \"answer\": \"Panels cut in opposite directions reflect light differently and show a shade shift at seams.\"\n    },\n    {\n      \"question\": \"When is a raised cloth over-finished?\",\n      \"answer\": \"When it pills, sheds or loses support, which is why pilling tests belong in the order.\"\n    }\n  ]\n}\n<\/script><\/p>\n<p><script type=\"application\/ld+json\">\n{\n  \"@context\": \"https:\/\/schema.org\",\n  \"@type\": \"FAQPage\",\n  \"mainEntity\": [\n    {\n      \"@type\": \"Question\",\n      \"name\": \"What is the difference between raising and brushing?\",\n      \"acceptedAnswer\": {\n        \"@type\": \"Answer\",\n        \"text\": \"Raising teases fibre out of the yarn with wire-covered rollers to create nap. Brushing lifts and aligns that nap and clears loose fibre.\"\n      }\n    },\n    {\n      \"@type\": \"Question\",\n      \"name\": \"Where does raising sit in the finishing line?\",\n      \"acceptedAnswer\": {\n        \"@type\": \"Answer\",\n        \"text\": \"After fulling, before shearing and the final stability steps such as pressing or decatizing.\"\n      }\n    },\n    {\n      \"@type\": \"Question\",\n      \"name\": \"Why must all panels be cut in one direction?\",\n      \"acceptedAnswer\": {\n        \"@type\": \"Answer\",\n        \"text\": \"A raised surface is directional. Panels cut in opposite directions reflect light differently and show a colour shift at the seam.\"\n      }\n    },\n    {\n      \"@type\": \"Question\",\n      \"name\": \"Does raising weaken the fabric?\",\n      \"acceptedAnswer\": {\n        \"@type\": \"Answer\",\n        \"text\": \"It reduces tear strength and can increase pilling, because fibre that supported the yarn structure is lifted to the surface.\"\n      }\n    },\n    {\n      \"@type\": \"Question\",\n      \"name\": \"How is a raised finish specified?\",\n      \"acceptedAnswer\": {\n        \"@type\": \"Answer\",\n        \"text\": \"By finish type and passes, faces, nap direction and shearing standard, plus a sealed reference sample and a pilling test requirement.\"\n      }\n    }\n  ]\n}\n<\/script><\/p>\n","protected":false},"excerpt":{"rendered":"<p>Two wool fabrics can leave the loom identical and arrive as different products. One is flat with the weave clearly readable, the other carries a soft surface where the structure sits behind a veil of fibre. The difference is not the yarn and not the weave; it is a pair of finishing steps, raising and &#8230; <a title=\"Raising and Brushing: How Nap Is Built in Wool Finishing\" class=\"read-more\" href=\"https:\/\/fursone.com\/sv\/raising-brushing-nap-finishing\/\" aria-label=\"L\u00e4s mer om Raising and Brushing: How Nap Is Built in Wool Finishing\">L\u00e4s mer<\/a><\/p>","protected":false},"author":1,"featured_media":2247,"comment_status":"open","ping_status":"open","sticky":false,"template":"","format":"standard","meta":{"rank_math_title":"Raising and Brushing in Wool Finishing | How Nap Is Built","rank_math_description":"Raising teases fibre to the surface; brushing lays it into a direction. Where these steps sit in the finishing line, what they change, and the risks an over-raised cloth carries.","rank_math_focus_keyword":"raising and brushing fabric finishing","rank_math_robots":"","rank_math_canonical_url":"","rank_math_facebook_title":"","rank_math_facebook_description":"","rank_math_twitter_title":"","rank_math_twitter_description":"","_yoast_wpseo_title":"","_yoast_wpseo_metadesc":"","_yoast_wpseo_focuskw":"","_yoast_wpseo_canonical":"","_yoast_wpseo_meta-robots-noindex":"","_yoast_wpseo_meta-robots-nofollow":"","_yoast_wpseo_opengraph-title":"","_yoast_wpseo_opengraph-description":"","_yoast_wpseo_twitter-title":"","_yoast_wpseo_twitter-description":"","_aioseo_title":"","_aioseo_description":"","_aioseo_keywords":"","_aioseo_robots_default":"","_aioseo_robots_noindex":"","_aioseo_og_title":"","_aioseo_og_description":"","_aioseo_twitter_title":"","_aioseo_twitter_description":"","aiosp_title":"","aiosp_description":"","aiosp_keywords":"","_seopress_titles_title":"","_seopress_titles_desc":"","_seopress_analysis_target_kw":"","_seopress_robots_canonical":"","_seopress_robots_index":"","_seopress_robots_follow":"","_seopress_social_fb_title":"","_seopress_social_fb_desc":"","_seopress_social_twitter_title":"","_seopress_social_twitter_desc":"","_genesis_title":"","_genesis_description":"","_genesis_canonical":"","_genesis_noindex":"","_genesis_nofollow":"","slim_seo":"","footnotes":""},"categories":[314],"tags":[],"class_list":["post-10616","post","type-post","status-publish","format-standard","has-post-thumbnail","hentry","category-production-craft"],"_links":{"self":[{"href":"https:\/\/fursone.com\/sv\/wp-json\/wp\/v2\/posts\/10616","targetHints":{"allow":["GET"]}}],"collection":[{"href":"https:\/\/fursone.com\/sv\/wp-json\/wp\/v2\/posts"}],"about":[{"href":"https:\/\/fursone.com\/sv\/wp-json\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"https:\/\/fursone.com\/sv\/wp-json\/wp\/v2\/users\/1"}],"replies":[{"embeddable":true,"href":"https:\/\/fursone.com\/sv\/wp-json\/wp\/v2\/comments?post=10616"}],"version-history":[{"count":0,"href":"https:\/\/fursone.com\/sv\/wp-json\/wp\/v2\/posts\/10616\/revisions"}],"wp:featuredmedia":[{"embeddable":true,"href":"https:\/\/fursone.com\/sv\/wp-json\/wp\/v2\/media\/2247"}],"wp:attachment":[{"href":"https:\/\/fursone.com\/sv\/wp-json\/wp\/v2\/media?parent=10616"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"https:\/\/fursone.com\/sv\/wp-json\/wp\/v2\/categories?post=10616"},{"taxonomy":"post_tag","embeddable":true,"href":"https:\/\/fursone.com\/sv\/wp-json\/wp\/v2\/tags?post=10616"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}