Reading Fabric Selvedge: Markings, Width and Quality Signals

D
Delia Fursone redaksjonsteam
Published on sep 21, 2026
4 min read

The selvedge, the finished edge running along both sides of a fabric roll, is the most information-dense strip on the goods, and most buyers step right over it. Woven into that few centimeters are the mill’s identity, the fabric’s usable width, the design’s repeat alignment and a set of quality signals you can read before cutting a sample. Learning to read the selvedge takes minutes and pays out across sourcing conversations, inspection days and dispute resolution. This guide walks through what is marked on the selvedge, what its condition tells you, and how to use it as evidence.

yarn threads on the weaving loom forming the fabric selvedge edge

Hva kanten tydelig forteller deg

Start med de trykte eller vevde merkingene. De fleste veverier merker merkevare- eller veverinavn, stoffets artikel- eller stilnummer, og noen ganger sammensetning og partiidentitet langs kanten; dette er sporbarbetsankerne du holder opp mot tilbud og følgesedler når rullene ankommer. Vepkanten er også der fargematchingskoder vises i enkelte programmer og knytter rullen tilbake til den godkjente labdipen. Hvis merkingen på leverte ruller ikke stemmer med papirene, er det ikke en trykkfeil; det er et brudd i sporbarbeten som rettferdiggjør å holde varene tilbake til veveriet forklarer byttet. Bredde, merket eller målbar mellom vepkantene, henger direkte sammen med forbruksberegningen, som vi bryter ned i veiledning for stoffbredde og stoffmengde.

Å lese kantens tilstand som et kvalitetssignal

The selvedge’s physical condition is a compressed quality report. A firm, even selvedge with no puckering indicates stable warp tension during weaving; wavy or drawn-in edges predict the same tension problems showing up as bowing or skew in the body. Loops or loose threads on the edge point to leno or selvedge-yarn issues that sometimes migrate into the first centimeters of usable width. Dye or print bleeding across the edge can foreshadow crocking problems in the body. None of these signals replaces a proper inspection; they tell you where to spend your inspection minutes, and they give inspectors a vocabulary for what they are seeing. The structured way to spend that time is the inspeksjonssystem med 4 poeng, som gjør kant- og stoffdefekter om til poengfradrag, og tankegangen bak defektklassifiseringen samsvarer med de standard test- og inspeksjonspraksisene som publiseres av organer som ASTM International for textile materials.

knit and tweed fabric swatches showing selvedge edges for quality comparison

Typer vepkant og hva de endrer i praksis

Not all edges are the same construction, and the type affects your cutting room. Woven selvedges with a chain or tuck-in finish are standard on quality wovens and tweeds, stable enough to sew or fold into the garment on premium goods. Knit fabrics come in tubular or slit-open forms, and the “selvedge” on open-width knits is a cut edge that demands immediate attention to curling. Fringed edges on some decorative wovens are intentional and should be quoted as such, not flagged as defects. Knowing the expected edge type for a construction prevents two opposite mistakes: rejecting an intentional edge, and accepting a sloppy one because it looked decorative.

Bruk av vepkanten i tvister og krav

Når en reklamasjon først oppstår, er kantlisten din bevispakke. Fotografer den i full lengde med merkingen synlig, sammen med rullmerket og fakturanummeret, før det gjøres noen kutting på rullen. Spenningsfeil, breddeavvik og avvik i merking kan alle dokumenteres tydelig fra kanten, og veverier løser reklamasjoner raskere når bevisene er entydige. Det er også derfor graderingssystemer for rullevarer registrerer kantfeil per rull; den Forklaring på rullgradering A, B og C viser hvordan kanttilstanden påvirker bokstaven en rull får. For innkjøpere som bygger en inspeksjonssjekkliste fra bunnen av, hører vevkantdelen hjemme ved siden av breddemålingen, og begge ligger inne i fabric sourcing guide arbeidsflyten vi bruker for innkommende varer.

Video: Stoffutvikling fra gulvet i partnerveveriet

▶Stoffer av høy kvalitet for designere

Ofte stilte spørsmål

Regnes vevskanten inn i den brukbare stoffbredden?

Nei. Brukbar bredde måles mellom sidelistene, og forbruksberegninger bør holde dem utenfor. Hull fra nåler, frynser og tyngre kantgarn gjør kanten ubrukelig i de fleste plagg.

Hvorfor har enkelte selvedger fargede tråder eller markeringer?

Fargede tråder og trykte koder inneholder vanligvis parti-, artikkel- eller matchingsinformasjon, slik at rullene kan spores gjennom kutting og reklamasjoner. Be veveriet om nøkkelen én gang, og kanten blir en lesbar loggbok.

Er en bølgete vepkant grunn til avvisning?

I seg selv ikke nødvendigvis; det avhenger av hva stoffet selv viser. Behandle det som en oppfordring til å inspisere for buing, skjevhet og spenningsfeil, og la deretter 4-poengsvurderingen avgjøre.

Hvordan bør jeg dokumentere vepkanten ved en reklamasjon?

Fotografer hele kanten med merkene synlige før kapping, sammen med rullappen og fakturanummeret. Entydig dokumentasjon av kanten gir raskere behandling hos veveriet i tvister om bredde, stramming og sporbarhet.