Heat-Set Pleats in Wool Tweed: What Must Be True?
Three conditions must hold before a pleater can set a pleat in wool tweed, and none of the three is a polyester percentage. First, the yarn carrying the thermoplastic component must be the yarn the ridge is pressed into. Second, the wool must be set by its own chemistry, because wool offers no melting point ... <a title="Heat-Set Pleats in Wool Tweed: What Must Be True?" class="read-more" href="https://fursone.com/heat-set-pleats-wool-tweed-what-must-be-true/" aria-label="Read more about Heat-Set Pleats in Wool Tweed: What Must Be True?">Read more</a>